Full annealing is one of the most fundamental heat-treatment processes applied to steels to ensure microstructural uniformity, improve ductility, reduce hardness, and restore workability.
To understand what is the result of full annealing of hypoeutectoid steels, it is essential to examine the metallurgical transformations occurring above and below the critical temperatures.
Hypoeutectoid steels contain 0.10% to 0.76% carbon, and their microstructure typically consists of ferrite (α-iron) and pearlite. These steels respond extremely well to full annealing, which makes them widely used in industrial fabrication where forming, machining, and shaping are required.
Understanding the Annealing Temperature Range
Full annealing is carried out by heating the steel to:
30–50°C above the A₃ temperature (upper critical point)
- A₃ varies according to carbon percentage:
- 910°C for 0.1% C
- Decreases gradually to 727°C as carbon approaches 0.76%
Heating above A₃ ensures 100% austenitization, meaning the entire microstructure transforms into austenite (γ-iron).
What Happens During the Process? (Step-by-Step Metallurgy)
1. Heating Stage
The steel is heated slowly to above the A₃ line. During this phase:
- Ferrite dissolves into austenite
- Pearlite transforms completely into austenite
- Carbon diffuses uniformly
- Grain boundaries begin to reorient
This creates homogeneous austenite, eliminating deformed grains created during forging or rolling.
2. Soaking Stage
At this stage, the steel is held at temperature long enough to allow:
- Full austenite homogenization
- Complete dissolution of prior microstructural phases
- Elimination of segregations
- Reduction of lattice distortions
Soaking time depends on the section thickness, typically 1 hour per 25 mm of thickness.
3. Slow Furnace Cooling
This is the most critical stage of full annealing. Cooling is intentionally slow:
- The furnace is switched off
- Steel is allowed to cool with the furnace
- Cooling rate typically: 20–30°C per hour
Slow cooling promotes equilibrium transformation, resulting in coarse pearlite and ferrite.
Detailed Results of Full Annealing of Hypoeutectoid Steels
Here is a deeper breakdown of the effects:
1. Formation of Ferrite + Coarse Pearlite (Final Microstructure)
During slow cooling:
- Austenite begins transforming around 727°C
- Low-carbon regions convert into ferrite
- Remaining austenite transforms into coarse pearlite
The final microstructure contains:
- Equiaxed ferrite grains
- Widely spaced lamellae in pearlite
- Reduced dislocation density
This structure is soft, ductile, and highly machinable.
2. Significant Reduction in Hardness
Typical hardness values before annealing:
- 150–220 BHN (depending on carbon content)
After full annealing:
- 90–130 BHN
The reduction occurs because coarse pearlite and ferrite require less force to deform compared to fine pearlite or bainite.
3. Major Improvement in Machinability
Annealed hypoeutectoid steels:
- Cut cleanly with less tool wear
- Produce longer, continuous chips
- Provide smoother surface finish
- Allow deeper cuts and higher feeds
Industries anneal these steels specifically to machine parts economically and efficiently.
4. Complete Removal of Internal Stresses
Manufacturing processes like:
- Hot rolling
- Cold drawing
- Forging
- Welding
- Punching
- Pressing
introduce severe residual stresses, making the material unpredictable during machining.
Full annealing:
- Stabilizes the lattice
- Eliminates internal stress patterns
- Prevents distortion during machining
- Improves dimensional accuracy
5. Grain Refinement and Improved Homogeneity
Annealing produces:
- Uniform, equiaxed grains
- Reduced grain-boundary energy
- Elimination of elongated grains formed during rolling
- Improved toughness and ductility
Grain refinement is crucial for impact-resistant applications.
6. Better Ductility and Formability
Annealed steels exhibit:
- Larger percent elongation
- Greater ability to undergo plastic deformation
- Higher bendability
- Better cold-forming characteristics
This makes them ideal for shaping operations such as:
- Deep drawing
- Stamping
- Press forming
- Wire drawing (after spheroidizing, if required)
7. Enhanced Microstructural Stability
Because the cooling is slow and controlled, the resulting microstructure is extremely stable, with minimal internal imbalance. This ensures better reliability during further heat treatment or fabrication.
Practical Industrial Uses After Full Annealing
Hypoeutectoid steels are fully annealed before manufacturing:
- Automotive components
- Flanges
- Shafts
- Gears (before hardening)
- Fasteners
- Base plates
- Pipe fittings
- Structural components
- Machine parts
Annealing ensures easier shaping and reliable performance.
Conclusion
To summarize what is the result of full annealing of hypoeutectoid steels : Full annealing produces a soft, ductile, stress-free microstructure consisting of ferrite and coarse pearlite.
It lowers hardness, improves machinability, enhances formability, refines grains, and restores structural uniformity.
This makes full annealing an essential pre-machining and pre-shaping treatment in industries using low- and medium-carbon steels.